What are typical starting temperatures for laminating with XinLi thermal laminating films?

What are typical starting temperatures for laminating with XinLi thermal laminating films?

The typical thermal adhesive will give good adhesion to lith-offset print at temperatures of 205 to 230*F (96 to 110*C). There are many factors in the laminating machine that have to be considered. Higher laminating speeds call for higher temperatures as
2020-03-26
What advantages do thermal lamination films offer for print finishing?

What advantages do thermal lamination films offer for print finishing?

XINLI  thermal lamination films also passed the SGS testing without any Toxic chemical composition involved , and are in compliance with the China environmental labeling standards calling for no pollution to the public with green production
2020-03-26
Production line retrofit surface inspection machine

Production line retrofit surface inspection machine

our company has introduced a set of film quality inspection equipment from the United States. The device's intelligent classification engine can accurately classify based on extremely small differences in defect categories
2020-04-11
What is "Silvering" and what can I do if it occurs?

What is "Silvering" and what can I do if it occurs?

Silvering is small air bubbles between the thermal adhesive and the printed substrate. These occur when the paper has greater roughness, insufficient pressure in the lamination nip or the laminating temperature is too low. Generally, the paper is already
2020-03-26
After laminating, can I immediately perform another operation such as embossing or creasing and folding?

After laminating, can I immediately perform another operation such as embossing or creasing and folding?

It is a good practice to let these warm sheets sit overnight to help set the interlaminar bond as they cool. It also helps hasten the curing of the litho-offset inks by oxidation. The problems can be a cohesive failure ink in that bond causing the laminat